Sunday, January 3, 2010

Blisters (Air Entrapment)

Blisters (Air Entrapment)

Description

Blisters are hollows created on or in the molded part. In contrast to a void (vacuum) this entrapped gas can also appear near the walls.

Possible Solutions

  • Decrease melt temperature.
  • Decrease screw speed.
  • Dry material.
  • Increase back pressure.
  • Increase mold temperature.
  • Ensure regrind is not too coarse.
  • Provide additional mold vents.
  • Relocate gate.

Brittleness

Description

Brittleness is a condition where the part cracks or breaks at a much lower stress level than would normally be expected based on the virgin material properties.

Possible Solutions

  • Check for material contamination.
  • Decrease amount of regrind use.
  • Decrease back pressure.
  • Decrease injection pressure.
  • Decrease screw speed.
  • Increase melt temperature.
  • Dry material. Refer to the drying instructions provided by the material supplier.