Description

Sprue Sticking generally occurs in a cold runner mold when the sprue is staying in the mold.

Possible Solutions

  • Check mold for undercuts and/or insufficient draft.
  • Decrease booster time.
  • Decrease injection pressure.
  • Decrease injection speed.
  • Decrease injection-hold.
  • Decrease mold close time.
  • Decrease nozzle temperature.
  • Increase core temperature.
  • Open the gates.
  • Ensure that the correct design of nozzle tip for the material is being used.