Sunday, January 3, 2010

Short Shot (Incomplete Filled Parts)

Short Shot (Incomplete Filled Parts)

Description

Short Shots occur when the part does not completely fill.

Possible Solutions

  • Increase back pressure.
  • Increase injection pressure.
  • Increase injection speed.
  • Increase melt temperature.
  • Increase mold temperature.
  • Increase nozzle temperature. Ensure that the manifold and nozzles have reached the set temperature.
  • Increase shot size and confirm cushion.
  • Make sure mold is vented correctly and vents are clear.
  • Confirm that the non-return valve used is not leaking excessively.
  • Increase the switch over pressure, distance, or time (whichever method is being used) point from fill to hold so the fill stage is used longer.
  • Change part design. Thin areas of the mold may not fill completely, especially if there is a thick to thin transition, or there is a long rib that cannot be vented very well. If the part design allows it, change in these areas can
    improve the situation.

No comments: